Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K Factor (ISO) | 3.0 µm/km @Temperature 200 °C |
3.0 µm/km @Temperature 392 °F |
|
Wolf Kunststoff ZEDEX® ZX-410 A4A Polymer Alloy ZX-410 is a bearing material with excellent properties and a very affordable price.Main Characteristics: Hard, Stiff, Tough; High dimensional stability; High chemical resistance; High water resistan.. |