Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, TD | 18.9 g/micron @Thickness 0.0400 mm |
480 g/mil @Thickness 0.00157 in |
ISO 6383-1 |
Total MDPE HF 513 Medium Density Polyethylene, Blown Film MDPE HF 513 is a medium density polyethylene produced by slurry loop low pressure process with hexene as co-monomer.MDPE HF 513 is a semi-high molecular weight polyethylene giving excellent mechanic.. |
|||
Elmendorf Tear Strength, TD | 18.9 g/micron @Thickness 0.0400 mm |
480 g/mil @Thickness 0.00157 in |
ISO 6383-2 |
Total MDPE HT 514 Medium Density Polyethylene, Blown Film MDPE HT 514 is a medium density polyethylene produced by slurry loop low pressure process with hexene as co-monomer.MDPE HT 514 is a semi-high molecular weight polyethylene giving excellent mechanic.. |