Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 5.52 MPa | 800 psi | chs 20 in/min; ASTM D412 |
Network Polymers Softflex® 0250 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 5.52 MPa | 800 psi | at 100%; ASTM D412 |
1085A Polyurethane-based Biomedical Elastomer |
|||
Tensile Strength, Yield | 5.52 MPa | 800 psi | ASTM D638 |
Global TPE-LS64A Elastomer Grade Data provided by Global Polymers Corporation. |
|||
Tensile Strength, Yield | 5.52 MPa | 800 psi | Elastic; ASTM D412 |
Multibase Multi-Flex® 8832 C Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Tensile Strength, Yield | 5.52 MPa | 800 psi | Elastic; ASTM D412 |
Multibase Multi-Flex® A 4001 LC TPE Thermoplastic Elastomer Features: Chemical Resistance, GoodCompressive Strength, GoodHeat Resistance, MediumOzone ResistantThermal Stability, GoodForms:PelletsProcessing Methods:Injection MoldingExtrusion Information pro.. |
|||
Tensile Strength, Yield | 5.52 MPa | 800 psi | Elastic; ASTM D412 |
Multibase Multi-Flex® A 4001 LCS Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Method:Injection Molding Information provided by Multibase |
|||
Tensile Strength, Yield | 5.52 MPa | 800 psi | Elastic; ASTM D412 |
Multibase Multi-Flex® A 5001 E LC Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection MoldingExtrusion Information provided by Multibase |
|||
Tensile Strength, Yield | 5.52 MPa | 800 psi | Elastic; ASTM D412 |
Multibase Multi-Flex® A 5001 LC Black TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, GoodWe.. |
|||
Tensile Strength, Yield | 5.52 MPa | 800 psi | Elastic; ASTM D412 |
Multibase Multi-Flex® A 5001 LC TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, GoodWe.. |
|||
Tensile Strength, Yield | 5.52 MPa | 800 psi | Elastic; ASTM D412 |
Multibase Multi-Flex® A 7727 E Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Tensile Strength, Yield | >= 5.52 MPa | >= 800 psi | Stress at Elongation M100; ASTM D412 Method A |
Seals Eastern 7265D Fluorocarbon-Elastomer Formulated Viton-ETP®. High temperature service in aggressive chemicals; Good base resistance.Information provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 5.52 MPa | 800 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3201-70 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling.. |
|||
Tensile Strength, Yield | 5.52 MPa | 800 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3211-70 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling.. |
|||
Tensile Strength, Yield | 5.52 MPa | 800 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3301-70 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To.. |
|||
Tensile Strength, Yield | 5.52 MPa | 800 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3310-75 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, RadiationUses-Automotive Applications, Food Service Applications, General Purpose, Med.. |
|||
Tensile Strength, Yield | 5.52 MPa | 800 psi | 100%; ASTM D412 |
Teknor Apex Flexalloy® 3501-65-NT Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MW, Ethylene Oxide SterilizableForms-PelletsProcessing-Extrusion, Injection MoldingAppe.. |
|||
Tensile Strength, Yield | 5.52 MPa | 800 psi | Tensile strength decreases by 15% after dry heat aging for 70 hrs at 437°F.; ASTM D412 |
Saint-Gobain COHRlastic® 300 General Purpose Silicone Solid Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
Tensile Strength, Yield | 5.52 MPa | 800 psi | ASTM D412-98 |
Saint-Gobain Tygon® 2001 Plasticizer Free Tubing Formulation Description: Tygon® 2001: Tygon® Plasticizer Free Tubing is a uniquely engineered product that offers the low compression set properties of a thermoset rubber. Tygon® Plasticizer Free Tub.. |
|||
Tensile Strength, Yield | 5.52 MPa | 800 psi | ASTM D412 |
Teknor Apex APEX® 3210-50 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge.. |
|||
Tensile Strength, Yield | 5.52 MPa | 800 psi | ASTM D412 |
Teknor Apex TEKBOND® 6700-55 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 5.52 MPa | 800 psi | ASTM D412 |
Teknor Apex UNIPRENE® 7400-64 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 5.52 MPa @Temperature 21.1 °C |
800 psi @Temperature 70.0 °F |
Flatwise Tensile |
Hexcel® Redux® 312UL Modified epoxy film adhesive Redux® 312 is a high-strength 250°F curing film adhesive, suitable for metal to metal bonding and sandwich constructions, where operating temperatures of up to 210°F may be experienced. A support.. |
|||
Tensile Strength, Yield | 5.52 MPa | 800 psi | ASTM D638 |
ExxonMobil Escorene® LD 713.93 Molding, extrusion and compounding resin Escorene Ultra LD 713.93 is a 14.4 wt% vinyl acetate copolymer with very good toughness, high clarity and excellent processability. It is suitable for use in making molded articles, extruded profile.. |
|||
Tensile Strength, Yield | 5.52 MPa | 801 psi | cured 60 mins @ 150°C |
ACC QLE 1039 QSI Quantum Silicones 40 Durometer Addition Cure Elastomer for Coating QLE 1039 is a 100% silicone solids elastomer designed for fabric or cloth coating applications. This two-component system offers a tough coating with excellent adhesion and fast cure.Key Features: .. |
|||
Tensile Strength, Yield | 5.52 MPa | 801 psi | cured |
ACC QLE 1101 QSI Quantum Silicones Specialty Silicone Coating QLE 1101 is a low viscosity, two-component, addition cure, silicone elastomer.Key Features: Fast cure at elevated temperaturesLow linear shrinkageTransparent, ideal for pigmentationLow viscosity Par.. |
|||
Tensile Strength, Yield | 5.52 MPa | 800 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3210-75 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge.. |
|||
Tensile Strength, Yield | 5.52 MPa @Strain 300 % |
800 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Monprene® MP 2356 Thermoplastic Elastomer Notes: Translucent Features: Excellent Chemical and Oil Resistance; Super Tough; Very Good Melt StrengthInformation Provided by Teknor Apex |
|||
Tensile Strength, Yield | 5.52 MPa @Strain 300 % |
800 psi @Strain 300 % |
Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® RT-3975 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerUV StabilizedNaturalApplications:Multi-PurposeMarket:AutomotiveBuilding and ConstructionConsumer GoodsIndustrialProcessing Method:Injecti.. |
|||
Tensile Strength, Yield | 5.52 MPa | 800 psi | TM R050-36 |
Resinlab® EP1282 Clear Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP1282 Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It is recognized under the Component Recognition Program of Underwriters Laborat.. |
|||
Tensile Strength, Yield | 5.52 MPa | 800 psi | TM R050-36 |
Resinlab® EP1296 Highly Filled, Moderately Thixotropic Black Casting Resin Resinlab™ EP1296 is a highly filled, moderately thixotropic black casting resin designed for applications requiring good thermal conductivity, low shrinkage and a low CTE. It was especially formula.. |