Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 480 - 660 MPa | 69600 - 95700 psi | |
Materion Beryllium Copper Alloy 190 Strip; AM (TM00) Temper (UNS C17200) Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 97%Stress Relaxation after 1000 hrs @ 200°C: 67%Formability Ratio, 90° Bend, R.. |
|||
Tensile Strength, Yield | 510 - 660 MPa | 74000 - 95700 psi | |
Materion Beryllium Copper Alloy 25 Strip; 1/2H (TD02) Temper (UNS C17200) Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0.5Formability Ratio (bad Way): 1Superficial Hardness: 30T 74-79Tabulated properties appl.. |
|||
Tensile Strength, Yield | 610 - 660 MPa @Strain 0.200 % |
88500 - 95700 psi @Strain 0.200 % |
|
CLAL-MSX DECLAFOR® 1015 TD4 Wire quenched/Cold Rolled Copper Alloy Main Characteristic: Age hardening alloyBeriyllium free alloyGood machinabilityHigh mechanical propertiesTypical Applications:Coaxial connectorsSpectacles partsSliding contacts partsAll kind of turn.. |