Polymer Property : Tensile Strength, Yield = 85000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 448 - 586 MPa

@Strain 0.200 %,
Thickness >=25.4 mm
65000 - 85000 psi

@Strain 0.200 %,
Thickness >=1.00 in
Turned Bars
Schmolz + Bickenbach 416 Stainless Steel Bar
Description: Ugitech’s 416 is free machining martensitic grade. The unique production process—developed exclusively by Ugitech—results in a product that delivers superior productivity..
Tensile Strength, Yield 503 - 586 MPa
73000 - 85000 psi
0.2% offset
Eagle Brass 425 Tin Brass 2%, Extra Hard
Alloy C425 is a low zinc-containing alloy with good combination of tensile strength, electrical conductivity, formability and corrosion resistance. Applications include electrical springs, connector..
Tensile Strength, Yield 483 - 586 MPa
70000 - 85000 psi
0.2% offset
Eagle Brass 521 Phosphor Bronzes 8% C, 3/4 Hard
Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical..
Tensile Strength, Yield 517 - 586 MPa

@Strain 0.200 %
75000 - 85000 psi

@Strain 0.200 %
Ametek AM 388™ Alloy (UNS C72650) TD03 3/4 Hard
Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and..
Tensile Strength, Yield 448 - 586 MPa

@Strain 0.200 %
65000 - 85000 psi

@Strain 0.200 %
Ametek High Purity Nickel Strip 899A 3/4 Hard
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..
Tensile Strength, Yield 448 - 586 MPa

@Strain 0.200 %
65000 - 85000 psi

@Strain 0.200 %
Ametek High Purity Nickel Strip 899L 3/4 Hard
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..
Tensile Strength, Yield 448 - 586 MPa

@Strain 0.200 %
65000 - 85000 psi

@Strain 0.200 %
Ametek High Purity Nickel Strip 899M 3/4 Hard
Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p..