Mechanical Properties Metric English Comments
Tensile Strength, Yield 30.4 - 55.9 MPa
4410 - 8110 psi
Average value: 44.4 MPa Grade Count:35
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m..