Polymer Property : Tensile Strength, Yield = 77000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 483 - 531 MPa
70000 - 77000 psi
0.2% offset
Eagle Brass 194 HSM® Copper, Extra Spring
High Strength Modified Copper Alloy C194 is a first generation high performance alloy used worldwide. C194 combines good electrical conductivity with high tensile strength, good solderability and pl..