Mechanical Properties Metric English Comments
Tensile Strength, Yield 34.5 - 49.6 MPa
5000 - 7200 psi
ASTM D-882
Saint-Gobain Norton® PVDF Fluoropolymer Film
Features/Benefits:Excellent weatherabilityHigh dielectric strengthExcellent chemical and abrasion resistanceThermoformableProduct available in widths up to 60"Product available with thicknesses from..