Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 276 - 483 MPa | 40000 - 70100 psi | |
Materion Beryllium Nickel Strip - Alloy 360 Annealed Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0Formability Ratio (bad Way): .. |