Mechanical Properties Metric English Comments
Tensile Strength, Yield 0.103 - 0.414 MPa
15.0 - 60.0 psi
Average value: 0.317 MPa Grade Count:5
Overview of materials for PVC, Foam Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Foam Grade". Each property range of values reported is minimum and maximum values of appropriate Ma..