Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 352 - 407 MPa | 51000 - 59000 psi | 0.2% offset |
Eagle Brass 151 ZHC® COPPER, Hard Alloy C151 has excellent solderability, high conductivity, and good strength. C151 has superior high temperature softening resistance compared to pure copper C110.Applications can be found in high c.. |
|||
Tensile Strength, Yield | 296 - 407 MPa | 43000 - 59000 psi | 0.2% offset |
Eagle Brass 18665 MSP1, 1/4 Hard MSP-1 high performance copper alloy with magnesium has high conductivity (63% IACS), high strength and excellent thermal creep properties. Typical uses include terminals, connectors, relays, springs.. |
|||
Tensile Strength, Yield | 303 - 407 MPa | 44000 - 59000 psi | 0.2% offset |
Eagle Brass 19210 XP-10 Copper Iron, 1/2 Hard 19210 has higher strengths than most copper alloys but thanks to its composition and processing it retains formability and conductivity that other copper alloys lose. Typical uses include cooling f.. |
|||
Tensile Strength, Yield | 110 - 407 MPa | 16000 - 59000 psi | 0.2% offset |
Eagle Brass 194 HSM® Copper, Annealed High Strength Modified Copper Alloy C194 is a first generation high performance alloy used worldwide. C194 combines good electrical conductivity with high tensile strength, good solderability and pl.. |
|||
Tensile Strength, Yield | 338 - 407 MPa | 49000 - 59000 psi | 0.2% offset |
Eagle Brass 220 Commercial Bronze, 3/4 Hard CDA 220 is known for having very good corrosion resistance, great cold workability and good hot workability for drawing, blanking, coining, stamping, piercing and punching. Typical uses include plum.. |