Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 200 - 380 MPa | 29000 - 55100 psi | |
Materion Beryllium Copper Alloy 25 Strip; A -Planished (TB00) Temper (UNS C17200) Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0Formability Ratio (bad Way): 0Superficial Hardness: 30T 46-67Tabulated properties apply .. |
|||
Tensile Strength, Yield | 170 - 380 MPa | 24700 - 55100 psi | |
Materion Brush 1915â„¢ Hard Temper Wire, 0.375" - 0.500" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Tensile Strength, Yield | 170 - 380 MPa | 24700 - 55100 psi | |
Materion Brush 1915â„¢ Hard Temper Rod, 0.375" - 0.500" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Tensile Strength, Yield | 220 - 380 MPa | 31900 - 55100 psi | |
Sinotek Materials CFC Carbon Heat Insulation Material Information provided by Sinotek |
|||
Tensile Strength, Yield | 290 - 380 MPa @Strain 0.200 % |
42100 - 55100 psi @Strain 0.200 % |
|
CLAL-MSX SICLANIC S® TD3 Quenched Copper Alloy, 1/2 Hard SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Tensile Strength, Yield | 300 - 380 MPa | 43500 - 55100 psi | |
ArcelorMittal Dual Phase 500 Very high strength steel, Cold Rolled Steel Available in the following: HCT600X (uncoated), HCT600X+ZE (electrogalvanized) and HCT600X+Z/ZF (Extragal®/Galvannealed)Description: Dual Phase steels offer an outstanding combination of strength a.. |
|||
Tensile Strength, Yield | 340 - 380 MPa | 49300 - 55100 psi | L direction |
ArcelorMittal Torque 20-15 Electrical Steel Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc.. |
|||
Tensile Strength, Yield | 340 - 380 MPa | 49300 - 55100 psi | L direction |
ArcelorMittal Torque 25-16 Electrical Steel Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc.. |
|||
Tensile Strength, Yield | 340 - 380 MPa | 49300 - 55100 psi | L direction |
ArcelorMittal Torque 27-16 Electrical Steel Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc.. |
|||
Tensile Strength, Yield | 340 - 380 MPa | 49300 - 55100 psi | L direction |
ArcelorMittal Torque 30-17 Electrical Steel Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc.. |
|||
Tensile Strength, Yield | 340 - 380 MPa | 49300 - 55100 psi | L direction |
ArcelorMittal Torque 30-18 Electrical Steel Properties: The iCARe™ Torque product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequenc.. |
|||
Tensile Strength, Yield | 300 - 380 MPa | 43500 - 55100 psi | |
ArcelorMittal FB 450 Hot rolled ferrite-bainite steel Available in the following: uncoated (HDT450F) and Extragal® (HDT450F+Z)Description: This range of hot-rolled high strength steels has been developed to meet weight reduction requirements. It compr.. |
|||
Tensile Strength, Yield | 300 - 380 MPa | 43500 - 55100 psi | |
ArcelorMittal FF 280 D Very high strength steel, Cold Rolled Steel Available in the following: HCT450X (uncoated), HCT450X+ZE (electrogalvanized) and HCT450X+Z/ZF (Extragal®/Galvannealed)Description: Dual Phase steels offer an outstanding combination of strength a.. |