Mechanical Properties Metric English Comments
Tensile Strength, Yield 37.0 - 37.0 MPa

@Temperature 80.0 - 80.0 °C
5370 - 5370 psi

@Temperature 176 - 176 °F
Average value: 37.0 MPa Grade Count:1
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo..
Tensile Strength, Yield 17.0 - 37.0 MPa
2470 - 5370 psi
Average value: 29.8 MPa Grade Count:12
Overview of materials for Polypropylene with 10% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Mica Filler". Specific grades with primary filler content between 5% and 14% are ..