Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 170 - 340 MPa | 24700 - 49300 psi | |
Materion Brush 1915™ AT Temper Wire Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°CBrush 1915™ is Brush Wellman's new heat-treatable leaded copper alloy. Enginee.. |
|||
Tensile Strength, Yield | 300 - 340 MPa | 43500 - 49300 psi | |
ArcelorMittal IF 300 High strength IF steel, Cold rolled Available in the following: Extragal®/Galvannealed (HX300YD+Z/+ZF)Description: These steels were designed to provide an excellent combination of drawability and mechanical strength based on their .. |
|||
Tensile Strength, Yield | 280 - 340 MPa | 40600 - 49300 psi | |
ArcelorMittal Dual Phase 450 Very high strength steel, Cold Rolled Steel Available in the following: HCT500X (uncoated), HCT500X+ZE (electrogalvanized) and HCT500X+Z (Extragal®/Galvannealed)Description: Dual Phase steels offer an outstanding combination of strength and .. |