Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 170 - 320 MPa | 24700 - 46400 psi | |
Materion Beryllium Copper Alloy 3 Plate & Rolled Bar; A (TB00) Temper; All Thicknesses (UNS C17510) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 170 - 320 MPa | 24700 - 46400 psi | |
Materion Beryllium Copper Alloy 10 Plate & Rolled Bar; A (TB00) Temper; All Thicknesses (UNS C17500) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 260 - 320 MPa @Strain 0.200 % |
37700 - 46400 psi @Strain 0.200 % |
|
SSAB Tunnplat Aluzink 260A RP-X High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Aluzink RP - rephosphorized steel (aluminum-zinc coated sheet). Property values are for thicknesses 0.5 - 1.5 mm. Iron content is approximate - exact compo.. |
|||
Tensile Strength, Yield | 260 - 320 MPa @Strain 0.200 % |
37700 - 46400 psi @Strain 0.200 % |
|
SSAB Tunnplat Docol® 260 RP High-strength Steel High-strength SteelComments: Docol RP - Cold Rolled Steel - rephosphorized steel. Property values are for cold-rolled steel; thicknesses 0.40 - 3.0 mm. Iron content is approximate - exact compositi.. |
|||
Tensile Strength, Yield | 250 - 320 MPa @Strain 0.200 % |
36300 - 46400 psi @Strain 0.200 % |
|
SSAB Tunnplat Docol® 400DP High-strength Steel High-strength SteelComments: Docol DP - Cold Rolled Steel - dual-phase steel. Property values are for cold-rolled steel; thicknesses 0.5 - 1.6 mm. Iron content is approximate - exact composition is.. |
|||
Tensile Strength, Yield | 260 - 320 MPa @Strain 0.200 % |
37700 - 46400 psi @Strain 0.200 % |
|
SSAB Tunnplat Dogal 260 RP High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Dogal RP - rephosphorized. Iron content is approximate - exact composition is not reported by the manufacturer.Data provided by SSAB Tunnplat. |
|||
Tensile Strength, Yield | 260 - 320 MPa @Strain 0.200 % |
37700 - 46400 psi @Strain 0.200 % |
|
SSAB Tunnplat Dogal 260 RP-X High-strength Metal-coated Steel High-strength Metal-coated SteelComments: Dogal RP - rephosphorized. Iron content is approximate - exact composition is not reported by the manufacturer.Data provided by SSAB Tunnplat. |
|||
Tensile Strength, Yield | 260 - 320 MPa | 37700 - 46400 psi | |
ArcelorMittal H 260 Solid solution steel, Cold rolled Available in the following: uncoated (HC260P) and electrogalvanized (HC260P+ZE) Description: Solid solution steels are designed to provide high strength while maintaining good drawability. These ste.. |
|||
Tensile Strength, Yield | 260 - 320 MPa | 37700 - 46400 psi | |
ArcelorMittal HSLA 260 High strength low alloy steel for cold forming, Cold Rolled Available in the following: uncoated (HC260LA), electroglavanized (HC260LA +ZE) and Extragal®/galfan/Galvannealed (HC260LA+Z/+ZA/+ZF)Description: Steels in the HSLA (High Strength Low Alloy) range .. |