Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 148 - 285 MPa | 21500 - 41300 psi | Average value: 223 MPa Grade Count:23 |
Overview of materials for Nylon 66, 60% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. .. |