Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 17.9 - 26.6 MPa | 2600 - 3860 psi | Average value: 22.1 MPa Grade Count:30 |
Overview of materials for High Density Polyethylene (HDPE), Rotational Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Rotational Molding Grade". Each property range of values reported is m.. |