Mechanical Properties Metric English Comments
Tensile Strength, Yield 21.6 - 23.5 MPa
3130 - 3410 psi
ASTM D1708
Polimersan Plastics POLITEF® (PTFE) with 15% Glass
As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv..
Tensile Strength, Yield 21.6 - 23.5 MPa
3130 - 3410 psi
ASTM D1708
Polimersan Plastics POLITEF® (PTFE) with 15% Glass
As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv..
Tensile Strength, Yield 16.0 - 23.5 MPa
2320 - 3410 psi
Average value: 19.2 MPa Grade Count:6
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded