Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 145 - 225 MPa | 21000 - 32600 psi | Average value: 186 MPa Grade Count:10 |
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are.. |