Polymer Property : Tensile Strength, Yield = 250200 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1715 - 1725 MPa

@Strain 0.200 %
248700 - 250200 psi

@Strain 0.200 %
Latrobe Marvac 250 VIM-VAR ; 10 in. High Strength Maraging Steel
MARVAC 250 VIM-VAR is a low carbon maraging steel capable of 240,000 psi minimum yield strength, coupled with excellent toughness and ductility. The alloy has good fabrication characteristics, which..