Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1.08 - 1.27 MPa | 157 - 184 psi | |
ACC EP IS EPI Engineered Polymers Integral Skin Flexible Foam EP-IS is integral skin flexible foam, “Powered by Reactamine ® Technology”, designed to give excellent surface skin. EP-IS contains cyclopentane as its blowing agent, which conforms to EPA standa.. |