Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 42.0 - 98.1 MPa | 6090 - 14200 psi | Average value: 67.9 MPa Grade Count:17 |
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar.. |
|||
Tensile Strength, Yield | 37.2 - 97.9 MPa | 5400 - 14200 psi | Average value: 71.3 MPa Grade Count:10 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant". Each property range of valu.. |
|||
Tensile Strength, Yield | 30.0 - 98.0 MPa | 4350 - 14200 psi | Average value: 72.2 MPa Grade Count:209 |
Overview of materials for Nylon 66, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Tensile Strength, Yield | 60.0 - 98.0 MPa | 8700 - 14200 psi | Average value: 72.5 MPa Grade Count:6 |
Overview of materials for Nylon, Amorphous Transparent Alloy This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Amorphous Transparent Alloy". Each property range of values reported is minimum and maximum value.. |