Polymer Property : Tensile Strength, Yield = 138000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 700 - 950 MPa

@Strain 0.200 %
102000 - 138000 psi

@Strain 0.200 %
SSAB Tunnplat Docol® 1000 DP High-strength Steel
High-strength SteelCharacteristics: The steels are annealed at temperatures between 750°C and 850°C, depending on the grade of steel, and then are hardened by quenching in water. Tempering is..
Tensile Strength, Yield 750 - 950 MPa
109000 - 138000 psi
ArcelorMittal Complex Phase Steel 1000 SF Very high strength steel, Cold Rolled Steel
Description: The Complex Phase family of steels supplements ArcelorMittal's VHSS (very high strength steel) product range. These steels are cold formed to make lightweight structural elements. A num..
Tensile Strength, Yield 800 - 950 MPa
116000 - 138000 psi
ArcelorMittal Complex Phase Steel 1000 Very high strength steel, Hot Rolled Steel
Available in the following: Extragal®/Galvannealed (HCT950C+Z)Description: The Complex Phase family of steels supplements ArcelorMittal's VHSS (very high strength steel) product range. These steels..
Tensile Strength, Yield 800 - 950 MPa
116000 - 138000 psi
ArcelorMittal Complex Phase Steel 1000 Y800 Very high strength steel, Cold Rolled Steel
Description: The Complex Phase family of steels supplements ArcelorMittal's VHSS (very high strength steel) product range. These steels are cold formed to make lightweight structural elements. A num..