Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 68.0 MPa | 9860 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CX7010 PC+ABS Cycoloy* CX7010 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0. Excellent flow combined with good balance of pro.. |
|||
Tensile Strength, Yield | 68.0 MPa | 9860 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® 4704 PPC High heat resistant polycarbonate copolymer, provides DTUL of 300F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with .. |
|||
Tensile Strength, Yield | 68.0 MPa | 9860 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® HFD4211 PC (Asia Pacific) Lexan* HFD4211 is a 10% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
Tensile Strength, Yield | 68.0 MPa | 9860 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® CFR5630D PC COPOLYMER (Europe-Africa-Middle East) LEXAN™ CFR5630D Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density a.. |
|||
Tensile Strength, Yield | 68.0 MPa | 9860 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® HFD4211 PC (Europe-Africa-Middle East) Lexan* HFD4211 is a 10% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
Tensile Strength, Yield | 68.0 MPa | 9860 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® LUX7630C PC COPOLYMER Lexan* LUX7630C Polycarbonate (PC) resin is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm.. |
|||
Tensile Strength, Yield | 68.0 MPa | 9860 psi | 50mm/min; ASTM D638 |
LG Chemical Lupoy 1320C-07 Polycarbonate Resin Description: LUPOY PC 1320C-07 resin provides stability against ultraviolet radiations to solid or multi-wall sheets via the coextrusion of a 50 ? thick layerMain Characteristics: Proprietary formul.. |
|||
Tensile Strength, Yield | 68.0 MPa | 9860 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Lubricomp GX07409X PSU Wear resistant PSUThis data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 68.0 MPa | 9860 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem ATX100R PEI+PCE Higher impact, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 HB listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 68.0 MPa | 9860 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem HATX100 PEI+PCE Higher impact, high flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
Tensile Strength, Yield | 68.0 MPa | 9860 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem HATX100 PEI+PCE (Europe-Africa-Middle East) Higher impact, high flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
Tensile Strength, Yield | 68.0 MPa | 9860 psi | 50mm/min; ISO 527 |
Teijin Multilon DN-1520B Filler Reinforced Type, Halogen-Free Flame Resistant PC/ABS Polymer Alloy Halogen-free flame retardant PC/ABS polymer alloy, and is also antimony-free. It has improved stiffness through the addition of 20 % filler. Improved stiffness and high fluidity realizes a thin wall.. |
|||
Tensile Strength, Yield | 68.0 MPa | 9860 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK500 PC+ABS (Asia Pacific) 10% GR, ECO conforming FR, PC+ABS for thinwall molding applications. |
|||
Tensile Strength, Yield | 68.0 MPa | 9860 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL NH5120C PPE+PS Noryl* NH5120C resin is a modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, good chemical resistance, and low specifc gravity for light weight parts. The .. |
|||
Tensile Strength, Yield | 68.0 MPa | 9860 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM STM1700 PEI Copolymer (Europe-Africa-Middle East) Siltem STM1700 is a flexible copolymer designed for wire and cable applications. It offers a halogen free (according VDE 0472) flame retardant solution that also offers low smoke emission and toxici.. |
|||
Tensile Strength, Yield | 68.0 MPa | 9860 psi | ISO 527-1/-2 |
Covestro Apec® 1695 Polycarbonate Easy flowingeasy to demoldsoftening temperature (VST/B 120)=158 °CPreprocessingMax. Water content |
|||
Tensile Strength, Yield | 68.0 MPa | 9860 psi | 50 mm/min; ISO 527-1,-2 |
Covestro Bayblend® FR3005 HG PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Tensile Strength, Yield | 68.0 MPa | 9860 psi | ISO 527-1/-2 |
Covestro Makrolon® 6717 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFLR,(,,)-05-9Global gradeFormerly Makrolon DP1-1853MVR (300 °C/1.2 kg) 3.0 cm3/10 minFlame retardantUL 94V-0/2.0 mmHigh viscosityBranchedUV stabilizedEasy releaseInjection molding - Me.. |
|||
Tensile Strength, Yield | 68.0 MPa | 9860 psi | 23°C, 50% RH; ASTM D638 |
Asahi Kasei Xyron® A0210 PPE/PA AutomotiveInformation provided by Asahi Kasei |
|||
Tensile Strength, Yield | 68.0 MPa | 9860 psi | ISO 527-1/-2 |
Covestro Makrolon® Rx1452 Polycarbonate ISO 7391-PC,M,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minMedical devicesLipid resistantsuitable for sterilization with high-energy radiationComplies with the requirements of FDA-modifie.. |
|||
Tensile Strength, Yield | 68.0 MPa | 9860 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® LUX7636C PC COPOLYMER (Asia Pacific) Lexan* LUX7636C Polycarbonate (PC) resin is a non-filled, extrudable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is U.. |