Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 675 MPa @Strain 0.200 % |
97900 psi @Strain 0.200 % |
|
Carpenter Gall-Tough PLUS™ Stainless, Annealed, 20% Cold Work Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r.. |
|||
Tensile Strength, Yield | 675 MPa @Strain 0.200 % |
97900 psi @Strain 0.200 % |
|
Haynes 25 alloy, room temperature after 10% cold reduction, 1065°C anneal for 5 minutes Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal gall.. |