Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 655 MPa | 95000 psi | |
Pacific Sintered Materials F-244-S(HT) High Carbon Steel Powdered Metal Applications:Highly stressed mechanical componentsGood hardenabilityEquivalent MPIF Specification: F-0008-85(HT)All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Yield | 655 MPa @Temperature -53.9 °C |
95000 psi @Temperature -65.0 °F |
0° Direction, Dry; ASTM D638 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Tensile Strength, Yield | 655 MPa @Strain 0.200 % |
95000 psi @Strain 0.200 % |
|
Hogen HM1250 Tungsten-Based Metal Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a low CTE which combine to resist thermal fatigue. The high melting point reduce.. |
|||
Tensile Strength, Yield | 655 MPa @Strain 0.200 % |
95000 psi @Strain 0.200 % |
|
Mi-Tech Metals Super Chatter Freeâ„¢ HD17.7 Tungsten-Based Metal Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a low CTE which combine to resist thermal fatigue. The high melting point reduce.. |
|||
Tensile Strength, Yield | 655 MPa @Strain 0.200 % |
95000 psi @Strain 0.200 % |
|
Haynes 214® alloy, 40% cold reduction, 925°C for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Tensile Strength, Yield | 655 MPa @Strain 0.200 % |
95000 psi @Strain 0.200 % |
|
Haynes 214® alloy, 50% cold reduction, 980°C (1800°F) for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Tensile Strength, Yield | 655 MPa | 95000 psi | 5 inches; Un-Nitrided |
Latrobe LSSâ„¢ 135M Nitriding Steel (ASTM A355 Class A) TLS 135M Nitriding Steel is a high-aluminum and chromium modification of AISI 4140 alloy steel. The aluminum addition promotes the formation of aluminum nitride compounds when tools manufactured fr.. |
|||
Tensile Strength, Yield | >= 655 MPa @Strain 0.200 %, Diameter 6.35 mm |
>= 95000 psi @Strain 0.200 %, Diameter 0.250 in |
CWSR; DAN 2700.9 |
Haynes Ti-3Al-2.5V Alloy Titanium Tubing Haynes® Ti-3Al-2.5V alloy is both lightweight and strong, providing a major design advantage - saving weight.Specific alloying additives, notably aluminum, raise the temperature at which a titani.. |
|||
Tensile Strength, Yield | 655 MPa @Strain 0.200 % |
95000 psi @Strain 0.200 % |
|
Haynes Ultimet® alloy, all-weld metal, GTAW weld Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Tensile Strength, Yield | 655 - 790 MPa | 95000 - 115000 psi | |
Materion Brush 60™ 3/4 HT Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 96%Stress Relaxation afte.. |
|||
Tensile Strength, Yield | >= 655 MPa | >= 95000 psi | |
MetalTek IN® 100 UNS N13100 Centri-Vac Nickel Based Alloy Information provided by MetalTek |
|||
Tensile Strength, Yield | 655 MPa @Strain 0.200 % |
95000 psi @Strain 0.200 % |
|
Haynes 25 alloy, room temperature sheet after 2500 hours of 650°C exposure Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Tensile Strength, Yield | 655 - 779 MPa | 95000 - 113000 psi | 0.2% offset |
Eagle Brass 64725 MAX251C, Spring Max 251c has an excellent balance in hardness, formability and conductivity. Typical uses include lead frames, circuit breakers, connectors, electrical springs, contact terminals, and fuse clips.In.. |
|||
Tensile Strength, Yield | >= 655 MPa | >= 95000 psi | 0.2% offset |
Eagle Brass 70265 XP175, 3/4 Hard Information provided by Eagle Brass Company |
|||
Tensile Strength, Yield | >= 655 MPa | >= 95000 psi | 0.2% offset |
Eagle Brass 752 Nickel Silver 18%, Extra Spring Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info.. |
|||
Tensile Strength, Yield | 655 MPa | 95000 psi | |
Chicago Extruded Metals BioBrass® UNS C95520 As-Cast Aluminum Bronze This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extruded Metals |
|||
Tensile Strength, Yield | 655 MPa | 95000 psi | Drawn rod and bar |
CMW® 100 Copper Alloy CMW® 100 material is a heat treatable, high strength, high conductivity copper base alloy. Its properties are a combination of highest strength and hardness with relatively high electrical and ther.. |
|||
Tensile Strength, Yield | 655 MPa | 95000 psi | |
CMW® THERMKON® 65M Molybdenum Copper parts For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc. |
|||
Tensile Strength, Yield | 655 MPa @Strain 0.200 % |
95000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum Grade 18 Titanium (UNS R56322) Uses: heat exchangers, industrial components, tubing.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum. |
|||
Tensile Strength, Yield | 655 MPa @Strain 0.200 % |
95000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum Grade 9 Titanium (UNS R56320) Uses: heat exchangers, industrial components, tubing.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum. |
|||
Tensile Strength, Yield | 655 MPa @Strain 0.200 % |
95000 psi @Strain 0.200 % |
|
ATI Allvac® Nickelvac® K-500 UNS N05500 Nickel Superalloy Uses: Pump and drive shafts, impellers, valve components, springs, fasteners, oil well packers, subsurface safety valves.Property values are for samples in the metallurgical condition: 1600°F annea.. |
|||
Tensile Strength, Yield | 655 MPa @Strain 0.200 % |
95000 psi @Strain 0.200 % |
|
ATI Allvac® Nickelvac® X-750 Nickel Superalloy, Heat Treatment: 1149°C (2100°F) + Age Data provided by Allvac.Applications: Turbine, engine components. Blades, vanes, fasteners, springs, bellows. Extrusion dies, nuclear, heat treating, forming tools. |