Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 65.5 MPa | 9500 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ NN-000/15T Polyamide 66 (Nylon 66) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Stat-Tech™ AS-08CF/000 UV FR V0 Acrylonitrile Butadiene Styrene (ABS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Polymer Resources PC/TP-GP2-G10 PC/Polyester Alloy, 10% Glass Reinforced Excellent Chemical Resistance, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information p.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
PTS Trimid® N66-1010 Utility Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® 5209 Black 30 A 1 Acetal (POM) Copolymer The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® 5209 Natural 1 Acetal (POM) Copolymer The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Ravago Manufacturing Americas Hylon® N1000THLUV2 Polyamide 66
(discontinued **) Available in North America Additive: Heat Stabilizer, Lubricant and UV StabilizerFeatures: Lubricated, Heat Stabilized and Good ToughnessRoHS CompliantAuto Specifications: GM GMP.PA66.079 Color: Bla.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Fiberfil® J-60/20/E/NS Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled, NSF listed Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | .01% permanent set |
Meehanite GF-20 Flake Graphite Cast Iron Type GF-20 is designed principally for high machinability and is used where ultimate strength is not an important factor.General Meehanite information - Meehanite metal is first melted to a definite.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Techmer ES HiFill FR® PA6 FR-N HS Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and LubricatedInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Techmer ES HiFill FR® PA6/6,6 GF NAT Availability: North AmericaForms: PelletsFeatures: Flame RetardantAppearance: Natural ColorProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Techmer ES HiFill® PA12 Availability: North AmericaForms: PelletsFeatures: Low ViscosityTPCI# 8807105Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Star Plastics ABSGF30 Molding Grade ABS With 30% Glass Information provided by Star Plastics, Inc. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Techmer ES HiFill® PP G/CF40 CC 40% Glass/Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Carbon Fiber Reinforcement, 40% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Techmer ES Luriblend® PA6 TS18 Nylon 6 Availability: North AmericaForms: PelletsAdditive: PTFE+ Silicone Lubricant(18%)Features: LubricatedInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Techmer ES Luriblend® PA6/6 TS18 Nylon 66 Availability: North AmericaForms: PelletsAdditive: PTFE + Silicone Lubricant (18%)Features: LubricatedInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | 0.125 in, injection molded, unannealed; ASTM D638 |
Styron EMERGEâ„¢ 4731-13 Polycarbonate EMERGEâ„¢ PC 4731-13 advanced resin is formulated with 10% glass fiber and has an f1 rating by Underwriters Laboratories Inc. It provides good ignition resistance, rigidity, dimension stability .. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ MEGARAD 2081-6LR Polycarbonate Resin Overview: CALIBREâ„¢ 2081-6LR Polycarbonate resin was developed for medical applications requiring improved resistance to lipids over standard polycarbonate resins. When exposed to a 20% intralip.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Westlake Plastics Propylux® CN-F Polypropylene (conductive) Non-sloughing, carbon-fiber-filled material with good chemical resistance, and high strength and stiffness and good temperature resistance to 215F. This material is light weight, easily machined an.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ISO R527 type 1 |
Hexcel® HexPly® 913 125°C Curing Epoxy Matrix HexPly® 913 is a proven modified epoxy matrix with a low temperature cure cycle which exhibits outstanding environmental resistance, whilst retaining good hot/wet mechanical performance. This versa.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D 638 |
A. Schulman COMTUF® 5011 10% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | |
TriStar Ultracomp UC-400 Composite Bearing Ultracomp UC-400 - Designed for high loads, low speeds, impact and vibration applications. UC-400 has a MOS2 additive for salt water applications where cathodic reactions could occur. Excellent dry .. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Ensinger TECACRYL® TECACRYL® offers excellent weather resistance, high light transmission, high mechanical strength, high surface hardness and mar resistance, good melt flow rate, and versatile colorability due to cr.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Clariant Renol R66G13HSL Nylon 66, 13% Glass Fiber, Heat Stabilized, Lubricated, Economy Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Ensinger Hydel® PC-P ESD Polycarbonate (PC) HYDEL® PC-P ESD polycarbonate is a static dissipative thermoplastic product containing carbon powder. This material has good stiffness, excellent dimensional ability, and low outgassing properties.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Clariant Renol 6601M Nylon 66, Molybdenum Disulfide Lubricated Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Asahi Kasei Thermylene® P-20FG-1740 20% Glass Fiber Reinforced, Medium Impact Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ ES-000/15T Polyethersulfone, PTFE Lubricated
(discontinued **) Description/Features:PTFE LubricatedInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Techmer ES HiFill FR® PPO/HIPS MM20 IM FR 20% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 20% Filler by WeightAdditive: Impact Modifier Features: Flame Retardant and Impact ModifiedInformation provided by TP C.. |