Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 64.1 MPa | 9300 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Gravi-Tech™ GT6000-0023 Black Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Tensile Strength, Yield | 64.1 MPa | 9300 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ NN-000/10T Polyamide 66 (Nylon 66) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Strength, Yield | 64.1 MPa | 9300 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ PPR-20G Black Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Tensile Strength, Yield | 64.1 MPa | 9300 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ PPR-20G Nat Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Tensile Strength, Yield | 64.1 MPa | 9300 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Trilliant™ HC HC5210-0020 RS Natural Polypropylene Homopolymer (PP Homopolymer) Information provided by PolyOne |
|||
Tensile Strength, Yield | 64.1 MPa | 9300 psi | ASTM D638 |
Polymer Resources PPX-EN-FR3 Modified-PPO, V-1 Flame Retardant, Extrusion Grade Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte.. |
|||
Tensile Strength, Yield | 64.1 MPa | 9300 psi | ASTM D638 |
Polymer Resources PPX-FR3 Modified-PPO, V-1 Flame Retardant Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Tensile Strength, Yield | 64.1 MPa | 9300 psi | ASTM D638 |
PTS SAN-82TR SAN Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 64.1 MPa | 9300 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® 5230 Natural 1 Acetal (POM) Copolymer The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Tensile Strength, Yield | 64.1 MPa | 9300 psi | ASTM D638 |
LTL Color Compounds ColorRxâ„¢ PC-1000RX Biocompatible Polycarbonate A biocompatible, 10 melt grade of Polycarbonate for healthcare applications.All information provided by LTL Color Compounders, Inc. |
|||
Tensile Strength, Yield | 64.1 MPa | 9300 psi | ASTM D638 |
LTL Color Compounds ColorRxâ„¢ PC-1001A Antimicrobial Polycarbonate A 10 melt grade of Polycarbonate containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color Compounders.. |
|||
Tensile Strength, Yield | 64.1 MPa | 9300 psi | ASTM D638 |
LTL Color Compounds ColorRxâ„¢ PC-1002AF Food Grade Polycarbonate A biocompatible, 10 melt grade of Polycarbonate for healthcare applications, containing antimicrobial protection.All information provided by LTL Color Compounders, Inc. |
|||
Tensile Strength, Yield | 64.1 MPa | 9300 psi | ASTM D638 |
LTL Color Compounds ColorRxâ„¢ PC-1002ARX Biocompatible Polycarbonate A biocompatible, 10 melt grade of Polycarbonate for healthcare applications, containing antimicrobial protection.All information provided by LTL Color Compounders, Inc. |
|||
Tensile Strength, Yield | 64.1 MPa | 9300 psi | ASTM D638 |
LTL Color Compounds ColorRxâ„¢ PC-1005ARX Biocompatible Polycarbonate A biocompatible, 10 melt grade of Polycarbonate for healthcare applications, containing a high level of antimicrobial protection for FDA regulated medical devices.All information provided by LTL Col.. |
|||
Tensile Strength, Yield | 64.1 MPa | 9300 psi | ASTM D638 |
Techmer ES HiFill® POM HO UV Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: HomopolymerInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 64.1 MPa | 9300 psi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ MEGARAD 2081-22 Polycarbonate Resin Overview: CALIBREâ„¢ 2081-22 polycarbonate resin is a high-flow resin designed for injection molded medical parts. It is stabilized to reduce color shift associated with exposure to high energy r.. |
|||
Tensile Strength, Yield | 64.1 MPa | 9300 psi | ASTM D638 |
Chase Plastics CP Pryme® PC100RHF Polycarbonate Form: PelletsInformation provided by Chase Plastics. |
|||
Tensile Strength, Yield | 64.1 - 73.1 MPa @Temperature 22.8 °C |
9300 - 10600 psi @Temperature 73.0 °F |
ASTM D638 |
Ensinger TECAST™ Cast Nylon (PA) TECAST™ Cast Nylon reduces downtime in heavy equipment applications. It is a low cost alternative for many non-ferrous machined parts. It has self-lubricating qualities which provide for excellen.. |
|||
Tensile Strength, Yield | 64.1 - 73.1 MPa @Temperature 22.8 °C |
9300 - 10600 psi @Temperature 73.0 °F |
|
Ensinger TECAST VEKTON™ 6PB Nylon 6 (PA6) TECAST VEKTON™ 6PB cushion pads are used to dampen the shock load on the anvil of a pile hammer. Specially formulated from an impact-modified type 6 nylon, they combine the excellent strength of n.. |
|||
Tensile Strength, Yield | 64.1 MPa | 9300 psi | ASTM D638 |
Asahi Kasei Thermylene® P-20FG-1714 20% Glass Fiber Reinforced, Medium Impact Information provided by Asahi Thermofil |