Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 63.74 MPa | 9245 psi | chs 2 in/min; ASTM D638 |
Network Polymers SAN 280 Water Clear Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc. |