Polymer Property : Tensile Strength, Yield = 9203 psi
Polymer Property :
Tensile Strength, Yield =
9203 psi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
63.45
MPa
9203
psi
chs 2 in/min; ASTM D638
Network Polymers PC-1030L
Description: Polycarbonate Information provided by Network Polymers Inc.