Polymer Property : Tensile Strength, Yield = 92000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 634 MPa
92000 psi
HP Alloys Alloy C-276, 10% Cold Worked
10% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati..
Tensile Strength, Yield 634 - 745 MPa
92000 - 108000 psi
0.2% offset
Eagle Brass 510 Phosphor Bronzes 5% A, Spring
Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info..
Tensile Strength, Yield 634 - 717 MPa
92000 - 104000 psi
0.2% offset
Eagle Brass 511 Phosphor Bronzes 4%, Extra Spring
511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge..
Tensile Strength, Yield 634 - 738 MPa
92000 - 107000 psi
0.2% offset
Eagle Brass 521 Phosphor Bronzes 8% C, Extra Hard
Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical..
Tensile Strength, Yield 634 MPa

@Strain 0.200 %
92000 psi

@Strain 0.200 %
Carpenter Custom 450® Stainless Steel, Condition H1150 (Age Hardened 621°C)
Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T..
Tensile Strength, Yield 634 MPa

@Strain 0.200 %,
Temperature 427 °C
92000 psi

@Strain 0.200 %,
Temperature 801 °F
Carpenter Custom 450® Stainless Steel, Condition H1150 (Age Hardened 621°C)
Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T..