Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 627 MPa | 91000 psi | Typical |
Kinetics MIM K3 Heat Treat as Sintered K3 is a custom Mo-Fe alloy that provides improved fatigue properties over many other steel alloys while still maintaining good strength components, industrial or structural components and other appl.. |
|||
Tensile Strength, Yield | >= 627 MPa | >= 91000 psi | |
Kinetics MIM K3 Heat Treat as Sintered K3 is a custom Mo-Fe alloy that provides improved fatigue properties over many other steel alloys while still maintaining good strength components, industrial or structural components and other appl.. |
|||
Tensile Strength, Yield | 627 MPa | 91000 psi | ASTM D3039 |
Greene Tweed Orthetek® WF Polyketone, Continuous Woven Carbon Fiber Greene Tweed offers precision-molded thermoplastic components made from our high-performance Orthtek® composite materials for a variety of demanding medical and biotechnology applications. Ortht.. |
|||
Tensile Strength, Yield | 627 MPa | 91000 psi | ASTM D3039 |
Greene Tweed WR™ 575 PEEK, Bi-Directional Carbon Fiber Filled WR®575 is a thermoplastic composite consisting of bi-directionally oriented carbon fibers in a PEEK matrix. The excellent wear resistance and the fiber orientation of WR575 makes this material i.. |
|||
Tensile Strength, Yield | 627 MPa @Strain 0.200 %, Temperature 399 °C |
91000 psi @Strain 0.200 %, Temperature 750 °F |
hardened to 310 HB |
Bohler-Uddeholm HOLDER Pre-hardened Holder Tool Steel Chromium-molybdenum alloyed steelA pre-hardened steel with very good machinability supplied at ~300 HB for clamping and holding plates and blocks.Holder is characterized by: Excellent machinability.. |