Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 621 MPa @Strain 0.200 % |
90100 psi @Strain 0.200 % |
|
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 1.0 mm thick sheet Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and.. |
|||
Tensile Strength, Yield | 621 MPa | 90100 psi | Forgings |
CMW® 100 Copper Alloy CMW® 100 material is a heat treatable, high strength, high conductivity copper base alloy. Its properties are a combination of highest strength and hardness with relatively high electrical and ther.. |
|||
Tensile Strength, Yield | 621 MPa | 90100 psi | |
CMW® 3950 AMS-T-21014 ASTM B777 High Density Machinable Tungsten Uses: Radiation Shielding, High Mass, Gyro, Ordnance. Machinability is similar to gray iron.Information provided by CMW Inc. |
|||
Tensile Strength, Yield | 621 MPa | 90100 psi | |
CMW® THERMKON® 70M Molybdenum Copper parts For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc. |
|||
Tensile Strength, Yield | 621 - 689 MPa @Strain 0.200 % |
90100 - 99900 psi @Strain 0.200 % |
|
Ametek High Purity Nickel Strip 899A Full Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Yield | 621 - 689 MPa @Strain 0.200 % |
90100 - 99900 psi @Strain 0.200 % |
|
Ametek High Purity Nickel Strip 899L Full Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Yield | 621 - 689 MPa @Strain 0.200 % |
90100 - 99900 psi @Strain 0.200 % |
|
Ametek High Purity Nickel Strip 899M Full Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Yield | 621 MPa @Strain 0.200 % |
90100 psi @Strain 0.200 % |
|
ATI Allvac® Nickelvac® H-46 Specialty Steel, Heat Treatment: 1149°C (2100°F) Anneal Data provided by Allvac.Applications: Structural components for land-based turbine engines. Rings and structurals in jet engines. |
|||
Tensile Strength, Yield | 621 MPa @Strain 0.200 % |
90100 psi @Strain 0.200 % |
|
ATI Allvac® Vasco® 316-L Specialty Steel, Heat Treatment: 1038°C (1900°F) Anneal Data provided by Allvac.Applications: Jet engine components, exhaust manifold heat exchangers, chemical process equipment, semiconductor systems. |
|||
Tensile Strength, Yield | 621 MPa @Strain 0.200 % |
90100 psi @Strain 0.200 % |
|
ATI Allvac® Vasco® 410/403 Specialty Steel, Heat Treatment: 927°C (1700°F) Anneal Data provided by Allvac.Applications: Compressor blades, turbine parts. |
|||
Tensile Strength, Yield | 621 MPa @Strain 0.200 % |
90100 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum AL 13-8™ H 1050 Precipitation Hardening Alloy, Heat Treated at 1150°F Characteristics: excellent strength, high hardness, superior toughness, good corrosion resistance, good transverse toughness properties, strength and ductility can be tailored by varying the aging t.. |
|||
Tensile Strength, Yield | 621 MPa | 90100 psi | Age Hardened per AMS 5872D, 21°C |
ATI Allegheny Ludlum Altemp® 263 Nickel-Based alloy Characteristics: high strength up to 1500°F, oxidation resistance up to 2000°FInformation provided by Allegheny Ludlum |
|||
Tensile Strength, Yield | >= 621 MPa @Strain 0.200 % |
>= 90100 psi @Strain 0.200 % |
|
HP Alloys Nitronic® 60 Austenitic Stainless, Level 1 Cold Worked Level 1 Cold Worked applies to tensile properties of 0.25 to 4 in. sizes; other properties are typical of this alloy.Nitronic 60 is truly an all purpose metal. This fully austenitic alloy was origin.. |
|||
Tensile Strength, Yield | 621 MPa | 90100 psi | |
HP Alloys HPA COBALT Alloy 6B, Wear Resistant, (Co-Cr-W) (UNS R30016) Cobalt 6B is a cobalt based chromium, tungsten alloy for wear environments where seizing, galling and abrasion are present. 6B is resistant to seizing and galling and with its low coefficient of fri.. |
|||
Tensile Strength, Yield | >= 621 MPa @Strain 0.200 % |
>= 90100 psi @Strain 0.200 % |
|
HP Alloys Nitronic® 50 Austenitic Stainless, Level 1 Cold Worked Cold Worked applies to tensile values and are for 0.25" to 4" diameter samples; other properties are typical of this alloy.Nitronic® 50 Stainless Steel provides a combination of corrosion resistanc.. |