Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 620 MPa @Strain 0.200 % |
89900 psi @Strain 0.200 % |
|
Hogen Diemitechâ„¢ Tungsten-Based Metal Diemitech is a new tungsten-based material used for high temperature tooling, die casting, extrusion dies, hot upsetting, and electro brazing. It has a higher tungsten content than similar available.. |
|||
Tensile Strength, Yield | 620 MPa @Strain 0.200 % |
89900 psi @Strain 0.200 % |
|
Hogen HM3050 Tungsten-Based Metal Mil Spec T-21014D Class 3; ASTM B-777-99 Class 3; AMS T-21014 Class 3. Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a low CTE.. |
|||
Tensile Strength, Yield | 620 - 800 MPa | 89900 - 116000 psi | |
Materion Beryllium Copper Alloy 25 Strip; H (TD04) Temper (UNS C17200) Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 1Formability Ratio (bad Way): 2.9Superficial Hardness: 30T 79-83Tabulated properties appl.. |
|||
Tensile Strength, Yield | 620 - 870 MPa | 89900 - 126000 psi | |
Materion Beryllium Copper Alloy 25 Wire; 1/2H (TD02) Temper; 1.3-12.7 mm Diameter (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 620 - 870 MPa | 89900 - 126000 psi | |
Materion Beryllium Copper Alloy M25 Wire; 1/2H (TD02) Temper; 1.3-12.7 mm Diameter (UNS C17300) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Yield | 620 MPa @Strain 0.200 % |
89900 psi @Strain 0.200 % |
|
Mi-Tech Metals Diemitechâ„¢ Tungsten-Based Metal Diemitech is a new tungsten-based material used for high temperature tooling, die casting, extrusion dies, hot upsetting, and electro brazing. It has a higher tungsten content than similar available.. |
|||
Tensile Strength, Yield | 620 MPa @Strain 0.200 % |
89900 psi @Strain 0.200 % |
|
Mi-Tech Metals HD17BB Tungsten-Based Metal ASTM B-777-07 Class 1; Slightly Magnetic (HD17 is non-magnetic).Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a low CTE which combine to resist t.. |
|||
Tensile Strength, Yield | 620 MPa @Strain 0.200 % |
89900 psi @Strain 0.200 % |
|
Mi-Tech Metals HD18D Tungsten-Based Metal Mil Spec T-21014D Class 3; ASTM B-777-99 Class 3; ASTM B-777-07 Class 3; AMS T-21014 Class 3. Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers high thermal con.. |
|||
Tensile Strength, Yield | 620 MPa @Strain 0.200 % |
89900 psi @Strain 0.200 % |
|
Haynes 214® alloy, 20% cold reduction, 980°C (1800°F) for 5 minutes Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Tensile Strength, Yield | 620 MPa @Temperature 100 °C |
89900 psi @Temperature 212 °F |
Wet; EN2561 |
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, TVR380/26% Fiber Information provided by HexCel |
|||
Tensile Strength, Yield | 620 - 758 MPa @Strain 0.200 % |
89900 - 110000 psi @Strain 0.200 % |
|
Ametek AM 388™ Alloy (UNS C72650) TM02 Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and.. |
|||
Tensile Strength, Yield | 620 - 750 MPa | 89900 - 109000 psi | |
ArcelorMittal Complex Phase Steel 750 Very high strength steel, Hot Rolled Steel Available in the following: uncoated (HCT750C) and Extragal®/Galvannealed (HCT750C+Z)Description: The Complex Phase family of steels supplements ArcelorMittal's VHSS (very high strength steel) prod.. |
|||
Tensile Strength, Yield | 620 MPa | 89900 psi | |
Latrobe Nitralloy® 135 Modified VAC-ARC, 1.5 to 3 in Premium Nitriding Steel NITRALLOY 135 MODIFIED VAC-ARC steel is a low alloy nitriding grade with moderate hardenability. It has been designed to provide a high case hardness and to maintain its core strength during the nit.. |