Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 61.4 MPa @Thickness 3.17 mm |
8910 psi @Thickness 0.125 in |
|
KEP Kepital® F20 Acetal Copolymer Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 61.4 MPa | 8910 psi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ 891-10 Polycarbonate Resin Overview: CALIBREâ„¢ 891-10 Series provides superior ignition resistance in opaque applications. The CALIBRE 891-10 series products are available in 2 additive packages: CALIBRE 891: Mold release.. |
|||
Tensile Strength, Yield | 61.4 MPa | 8910 psi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ 893-10 Polycarbonate Resin Overview: CALIBREâ„¢ 893-10 Series provides superior ignition resistance in opaque applications. The CALIBRE 891-10 series products are available in 2 additive packages: CALIBRE 891: Mold release.. |