Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 590 MPa @Strain 0.200 % |
85600 psi @Strain 0.200 % |
|
Hogen HM3000 Tungsten-Based Metal Mil Spec T-21014D Class 3; ASTM B-777-99 Class 3; AMS T-21014 Class 3. Nil magnetic properties.Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a l.. |
|||
Tensile Strength, Yield | 590 MPa @Strain 0.200 % |
85600 psi @Strain 0.200 % |
|
Hogen HM3750 Tungsten-Based Metal Mil Spec T-21014D Class 4; ASTM B-777-99 Class 4; AMS T-21014 Class 4. Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a low CTE.. |
|||
Tensile Strength, Yield | 590 MPa @Strain 0.200 % |
85600 psi @Strain 0.200 % |
|
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 11.1 mm thick plate Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and.. |
|||
Tensile Strength, Yield | 590 MPa @Strain 0.200 % |
85600 psi @Strain 0.200 % |
|
Mi-Tech Metals HD18 Tungsten-Based Metal Mil Spec T-21014D Class 3; ASTM B-777-99 Class 3; ASTM B-777-07 Class 3; AMS T-21014 Class 3. Nil magnetic properties.Manufactured by powder metallurgy methods. The tungsten base offers high therm.. |
|||
Tensile Strength, Yield | 590 MPa @Strain 0.200 % |
85600 psi @Strain 0.200 % |
|
Mi-Tech Metals HD18.5 Tungsten-Based Metal Mil Spec T-21014D Class 4; ASTM B-777-99 Class 4; ASTM B-777-07 Class 4; AMS T-21014 Class 4. Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers high thermal con.. |
|||
Tensile Strength, Yield | >= 590 MPa | >= 85600 psi | |
SSAB Tunnplat Domex® 590XP Extra High-strength Cold-forming Steel Extra High-strength Cold-forming Steel, HSLACharacteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. Gene.. |
|||
Tensile Strength, Yield | 590 - 700 MPa @Strain 0.200 % |
85600 - 102000 psi @Strain 0.200 % |
|
CLAL-MSX SICLANIC S® TH4 Quenched Copper Alloy, 4/4 Hard, precipitation treated SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |