Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 586 MPa @Temperature 21.1 °C |
85000 psi @Temperature 70.0 °F |
0° Direction, Dry; ASTM D638 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 3K 8HS Carbon Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Tensile Strength, Yield | 586 MPa @Temperature 23.9 °C |
85000 psi @Temperature 75.0 °F |
0° Direction, Dry; ASTM D638 |
Park Electrochemical Nelcote® V-341 Polybutadiene Prepreg, 581 Quartz Reinforced Nelcote® V-341 is Polybutadiene resin system designed to provide excellent electrical properties in demanding airborne, shipboard, and undersea applications.Key Features and Benefits:Extremely low .. |
|||
Tensile Strength, Yield | 586 MPa | 85000 psi | Typical |
Kinetics MIM F1537 (ASTM F1537) HIP and Heat Treat Most commonly used within the medical market on applications requiring these characteristics: Bio-compatibility Corrosion resistance High strength Nonmagnetic Wear resistance. Information prov.. |
|||
Tensile Strength, Yield | >= 586 MPa @Diameter 3.17 - 88.9 mm, Strain 0.200 % |
>= 85000 psi @Diameter 0.125 - 3.50 in, Strain 0.200 % |
mid-radius; ASTM E-8 |
H.C. Starck Molybdenum Hafnium Carbide Powder, Metallurgy Alloy Bar MHC Description of Product: This specification covers molybdenum alloy (molybdenum + 1.2% hafnium) wrought bar produced from pressed and sintered metallurgy billet.Structure: The MHC alloy bars can be.. |
|||
Tensile Strength, Yield | 586 MPa @Strain 0.200 % |
85000 psi @Strain 0.200 % |
|
Haynes Ultimet® alloy, aged 1000 hours at 649°C (1200°F) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Tensile Strength, Yield | 586 MPa @Strain 0.200 % |
85000 psi @Strain 0.200 % |
|
Haynes Ultimet® alloy, all-weld metal, GMAW weld (spray) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Tensile Strength, Yield | 586 MPa @Strain 0.200 % |
85000 psi @Strain 0.200 % |
|
Haynes Hastelloy® C-22® alloy, GTAW, aged 4000 hours at 450°C (800°F), notched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Tensile Strength, Yield | 586 - 703 MPa | 85000 - 102000 psi | 0.2% offset |
Eagle Brass 510 Phosphor Bronzes 5% A, Extra Hard Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info.. |
|||
Tensile Strength, Yield | >= 586 MPa | >= 85000 psi | 0.2% offset |
Eagle Brass 7026 Copper Nickel, 1/2 Hard 7026 is a high performance alloy used in springs, terminals, elevated temperature interconnects and high reliability telecommunication components.Information provided by Eagle Brass Company |
|||
Tensile Strength, Yield | >= 586 MPa | >= 85000 psi | 0.2% offset |
Eagle Brass 70265 XP175, 1/2 Hard Information provided by Eagle Brass Company |
|||
Tensile Strength, Yield | 586 MPa | 85000 psi | |
CMW® 2000 AMS-T-21014 ASTM B777 High Density Machinable Tungsten Uses: Radiation Shielding, High Mass, Gyro, Ordnance. Machinability is similar to gray iron.Information provided by CMW Inc. |
|||
Tensile Strength, Yield | 586 MPa | 85000 psi | Typical |
Dura-Bar 100-70-03 Continuously Cast Ductile Iron Bar Stock ASTM A536 Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as a direct replacement for.. |
|||
Tensile Strength, Yield | 586 MPa @Strain 0.200 % |
85000 psi @Strain 0.200 % |
|
ATI Allegheny Ludlum AL 4466™ Ferritic Stainless Steel Low carbon, low nitrogen ferritic stainless steel alloy. Characteristics:outstanding resistance to chloride pitting and crevice corrosion, improved resistance over austenitic stainless steels to ch.. |
|||
Tensile Strength, Yield | 586 MPa @Strain 0.200 % |
85000 psi @Strain 0.200 % |
|
ATI Allvac® 3-2.5 Titanium Alloy, Heat Treatment: 704°C (1300°F) Anneal Data provided by Allvac.Applications: Excellent cold formability, 20-50% higher tensile properties than CP titanium grades. Primarily used in aircraft hydraulic systems. |
|||
Tensile Strength, Yield | 586 MPa | 85000 psi | |
HP Alloys Alloy 718, 5% Cold Worked 5% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internatio.. |
|||
Tensile Strength, Yield | 586 MPa @Strain 0.200 %, Temperature -73.0 °C |
85000 psi @Strain 0.200 %, Temperature -99.4 °F |
|
Carpenter Gall-Tough® Stainless, Annealed and Cold Drawn Bar, 10% Cold Work Data provided by Carpenter Technology Corporation.Threshold Galling Stress 103 MPa (higher stress tests not performed). The avg. total volume loss on the wear test is 5 mm³ at 100 rpm.Gall-Tough®.. |
|||
Tensile Strength, Yield | 586 - 669 MPa | 85000 - 97000 psi | 0.2% offset |
Eagle Brass 752 Nickel Silver 18%, Extra Hard Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info.. |