Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 58.0 MPa | 8410 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® C2800 PC+ABS Non-chlorinated and non-brominated flame retardant PC+ABS offering balanced flow and impact properties for various applications. |
|||
Tensile Strength, Yield | 58.0 MPa | 8410 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 201 PC (Asia Pacific) 7.0 MFR, for thicker sections without sinks. Improved flame retardance. |
|||
Tensile Strength, Yield | 58.0 MPa | 8410 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL1132T PC Copolymer (Asia Pacific) Lexan* EXL1132T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) .. |
|||
Tensile Strength, Yield | 58.0 MPa | 8410 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA. |
|||
Tensile Strength, Yield | 58.0 MPa | 8410 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA. |
|||
Tensile Strength, Yield | 58.0 MPa | 8410 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL9134 PC Copolymer Lexan* EXL9134 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high flow opaque injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, .. |
|||
Tensile Strength, Yield | 58.0 MPa | 8410 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® FXE1112T PC Copolymer Lexan* FXE1112T Lexan* polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high flow ch.. |
|||
Tensile Strength, Yield | 58.0 MPa | 8410 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® FXE1413T PC Copolymer (Europe-Africa-Middle East) Clear PC-siloxane copolymer with excellent processability, for Visual fX capability in "Energy" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color packa.. |
|||
Tensile Strength, Yield | 58.0 MPa | 8410 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® HPX4 PC Copolymer (Europe-Africa-Middle East) Medium flow specialty polycarbonate - improved processability & autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP.. |
|||
Tensile Strength, Yield | 58.0 MPa | 8410 psi | ASTM D 638 |
SABIC Innovative Plastics LNP Colorcomp D10009 PC (Asia Pacific) LNP* Colorcomp* D10009 is a compound based on Polycarbonate resin containing Flame Retardant, Unfilled Custom Color. Added features of this material include: Flame Retardant.This data was supplied .. |
|||
Tensile Strength, Yield | 58.0 MPa | 8410 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® EXL1112T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1112T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with high flow char.. |
|||
Tensile Strength, Yield | 58.0 MPa | 8410 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA. |
|||
Tensile Strength, Yield | 58.0 MPa | 8410 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL9330 PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA. |
|||
Tensile Strength, Yield | 58.0 MPa | 8410 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL9330 PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. Non-chlorinated, non-brominated flame retardant product in most colors. UV-stabilized. UL rated f1/V-0/5VA. |
|||
Tensile Strength, Yield | 58.0 MPa | 8410 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® X4820 PBT+PC (Asia Pacific) Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability. |
|||
Tensile Strength, Yield | 58.0 MPa | 8410 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Europe-Africa-Middle East) Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional .. |
|||
Tensile Strength, Yield | 58.0 MPa | 8410 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® X4810 PBT+PC (Asia Pacific) Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent.. |
|||
Tensile Strength, Yield | 58.0 MPa | 8410 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL 731 PPE+PS PPE+PS blend. Unfilled. NSF listed for potable water use in several colors (Standard 61). FDA compliant in several colors (restrictions apply). UL94 HB rated. Low water absorption. Hydrolytic stabi.. |
|||
Tensile Strength, Yield | 58.0 MPa | 8410 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL 731S PPE+PS (Asia Pacific) High heat PPO/HIPS alloy suitable for use in some potable water applications. |
|||
Tensile Strength, Yield | 58.0 MPa | 8410 psi | ASTM-D638 |
Polyram RamLloy PI300G6 PVDF, 30% Glass Fiber 30% glass fiber reinforced, high thermal resistance high UV and radiation PVDF for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 58.0 MPa | 8410 psi | ASTM D638 |
Eastman Eastar EN001 Copolyester Eastar EN001 Copolyester is a thermoplastic polyester copolymer. Eastar EN001 Copolyester has a relatively slow crystallization rate. This broadens the operating window for extrusion and forming pro.. |
|||
Tensile Strength, Yield | 58.0 MPa | 8410 psi | ASTM D 638 |
Cossa Polimeri ESTABLEND PSA 6600 PC / ASA Blend Polycarbonate and acrylonitrile styrene acrylate blendGood light resistance, good impact resistance, high heat resistance, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Tensile Strength, Yield | 58.0 MPa | 8410 psi | parallel; ISO 527-3 |
Covestro Desmopan® DP 3354D Polyurethane As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Tensile Strength, Yield | 58.0 MPa | 8410 psi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® FGS600F40 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Low Viscosity Polybutylene Terephthalate Developed for Food Contact Applications Crastin FGS600F40 NC010 is an unreinforced low viscosity polybutylene terephthalate resin for injection .. |
|||
Tensile Strength, Yield | 58.0 MPa | 8410 psi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® SC164 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Low Viscosity Polybutylene Terephthalate Developed for the Healthcare Industry Crastin SC164 NC010 is an unreinforced low viscosity polybutylene terephthalate resin for injection moldin.. |
|||
Tensile Strength, Yield | 58.0 MPa | 8410 psi | ISO 527 |
Azoty Tarnow™ TARNOFORM 500 UV POM High flow injection molding grade based on Tarnoform 500 modified with carbon black giving best weathering stability.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Tensile Strength, Yield | 58.0 MPa @Temperature 100 °C |
8410 psi @Temperature 212 °F |
|
BASF Ultrason S 3010 PSU Ultrason S 3010 is an unreinforced, higher viscosity injection molding and extrusion PSU grade, tougher and with improved chemical resistance. It conforms to FDA requirements of 21 CFR 177.1655. |
|||
Tensile Strength, Yield | 58.0 MPa | 8410 psi | GB/1040 |
Zhejiang Juner PC-A1-11 Top-Grade Flame Retardant UV-Resistant Applications: Top-Grade Wall Switch, BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |