Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 570 MPa @Strain 0.200 %, Temperature 650 °C |
82700 psi @Strain 0.200 %, Temperature 1200 °F |
|
Haynes 242® alloy, bar and rings, annealed and aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Tensile Strength, Yield | 570 MPa @Strain 0.200 % |
82700 psi @Strain 0.200 % |
|
Haynes 25 alloy, room temperature after 25% cold reduction, 1120°C anneal for 5 minutes Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Tensile Strength, Yield | 570 MPa @Strain 0.200 % |
82700 psi @Strain 0.200 % |
|
Haynes 556® alloy, 50% cold reduction, 1010°C anneal for 5 minutes Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Tensile Strength, Yield | 570 MPa @Strain 0.200 % |
82700 psi @Strain 0.200 % |
|
Haynes 625 alloy, 50% cold reduction, 1065°C anneal for 5 minutes Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Tensile Strength, Yield | 570 MPa | 82700 psi | Annealed |
Special Metals INCONEL® Alloy MA 754 A mechanically alloyed nickel-chromium alloy with oxide dispersion strengthening. Mechanical alloying, which involves high-energy milling of metal powders, is used to create a uniformly distributed.. |
|||
Tensile Strength, Yield | 570 MPa @Strain 0.200 % |
82700 psi @Strain 0.200 % |
Typical |
TIMET 100A CP Titanium Industry Specifications: USA Aerospace: AMS 4921. Germany Engineering: 3.7065. Germany Aerospace: 3.7064. France: T-60. UK Aerospace Specifications BS TA. 7, 8, 9.Features: The mechanical prope.. |