Tensile Strength, Yield 56.2 MPa
8150 psi
chs 2 in/min; ASTM D638
Network Polymers PC-1029 AS/P
Description: Antistatic PolycarbonateInformation provided by Network Polymers Inc.
Tensile Strength, Yield 56.2 MPa
8150 psi
ASTM D412
C.O.I.M. LARIPUR® LPR2203-93A Seal Grade TPU
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..