Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 56.0 MPa | 8120 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® MC8002 PC+ABS (Asia Pacific) AUTOMOTIVE. Low viscosity, high impact and ductility. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® XCM830 PC+ABS PC/ABS with high stiffness and impact performance |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® BM5225X PC (Asia Pacific) BM5225X resin is a mineral filled grade featuring of high modulus, good flow and ductility, low warpage. It is of non-Br & non-Cl flame retardant systems intended to meet thin wall flame resistance .. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXD9810 PC Copolymer (Asia Pacific) Non-chlorinated, non-brominated Flame retardant PC-siloxane copolymer blend. Excellent processability, super high flow, good impact, UL rated V-0. Limited translucent colors. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXE1414T PC Copolymer Clear PC-siloxane copolymer with excellent processability, for Visual fX capability in ""Energy"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color pac.. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXM1414T PC Copolymer (Asia Pacific) PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL1414H PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxan copolymer with excellent processability. Medium flow, extreme low temperature ductile. Enhanced hydrolytic stability. Only available in black color. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXD9810U PC Copolymer (Asia Pacific) Polycarbonate with high flow, excellent processability, good impact and thermal properties, UV stabilized, non-Chlorine and non-Bromine flame retardant, UL rated V-0 and V-1. Available in limited di.. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | ASTM D638M |
DSM Somos® 7110 Epoxy Photopolymer, UV Postcure
(discontinued **) DescriptionDSM Somos® 7110 Photopolymer is a humidity-tolerant, high heat-deflection-temperature, low-curl, high-speed liquid that produces rigid, highly accurate parts. It produces exceptional, u.. |
|||
Tensile Strength, Yield | 56.0 MPa @Temperature 22.0 °C |
8120 psi @Temperature 71.6 °F |
25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® SMC 1650 Unsaturated Polyester UP SMC 1650 is a specially designed anti-microbial polyester moulding compound which incorporates a "germ killer" . It has been tested and found to be compliant for resistance to fungal defacement in .. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON DX05301C PC LNP* STAT-KON* DX05301C is a compound based on Polycarbonate containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive, Low Ionic.. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® IQ3001 PBT (Asia Pacific) Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP DX09402 PC LNP* THERMOCOMP* DX09402 is a compound based on Polycarbonate containing Proprietary Filler(s). |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | ISO 527 |
SABIC Innovative Plastics LNP Thermotuf U1000AIS PPA (Asia Pacific) LNP* Thermotuf* U1000AIS is a compound based on Polyphthalamide resin. Added features of this material include: High Impact, Heat Stabilized.This data was supplied by SABIC-IP for the Asia Pacific .. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX GTX905 PPE+PS+PA Automotive. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Valox® 350U PBT (Asia Pacific) Impact modified, UV stabilised, flame retardant polyester with an internal glowwire rating of 850C on 1.6mm flat plaques.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | ASTM D638 |
SABIC Innovative Plastics LNP STAT-LOY NX03583 PC+ABS (Asia Pacific) LNP STAT-LOY* NX03583 is a compound based on PC+ABS Blend resin containing Anti-Static, Flame Retardant. Added features of this material include: Antistat. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® X5630 PC+PET Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applicationsThis data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 56.0 MPa @Temperature 23.0 °C |
8120 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® 954-3A Curing Cyanate Resin HexPly® 954-3A is a 350°F (177°C) curing cyanate resin with a 400°F (204°C) glass transition temperature. Standard cure is two hours at 350°F (177°C). Glass transition temperatures can be max.. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | 50 mm/min |
Eastman Eastar EN058 PET Copolymer ISO data as provided by the manufacturer, Eastman Chemical |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | chs 50 mm/min; ASTM D638 |
Diamond Polymers DIAMALOY PC 1113 Impact Modified Polycarbonate Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | ASTM D638 |
Engineered Plastics EP Alloy 510B PC/ABS Alloy Gray. Stiff tough and excellent color stability. Used in housings for computers, printers, copiers and for auto parts such as air ducts and instrument panels. GMP # 002; Ford # WSS585. Propert.. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | 50 mm/min; ISO 527-2 |
BASF Ultradur® B 6550 LN PBT Description: High-viscosity grades for the extrusion of loose buffer tubes for optical fibers, semi-finished products for machining, profiles and pipes.Information provided by BASF |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXE1434T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1434T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers extreme low temperature (-40 C) ductility in combination with me.. |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | ASTM D638 |
Fiberfil® J-68/30/E/UV Polypropylene Copolymer, 30% Glass Fiber Reinforced, Chemically coupled, UV Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Strength, Yield | 56.0 MPa | 8120 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON ME006 PP LNP STAT-KON* ME006 is a compound based on Polypropylene resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |