Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 55.0 MPa | 7980 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® C2800 PC+ABS (Europe-Africa-Middle East) Non-chlorinated and non-brominated flame retardant PC+ABS offering balanced flow and impact properties for various applications. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | ISO 527, ASTM D638 |
Nilit Nilitop BT FR C3 Unfilled, Flame Retardant PBT Description: Nilitop BT FR C3 is an unfilled, flame retardant PBT with halogens. The flame retardant does not contain PBB and PBDE, so it is compliant with the WEEE directive.Key characteristics: Go.. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® CY9640 PC+ABS (Asia Pacific) PC+ ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | 50 mm/min; ISO 527-1,2 |
Qualchem Danamid AFES-23 Polyamide 66 Impact resistant, coldInformation provided by Qualchem Zrt. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DL002F PC LNP LUBRICOMP* DL002F is a compound based on Polycarbonate resin containing 10% PTFE. Added features of this material include: Internally Lubricated, Superior Molding. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | 0.2 in/min; 0.050" thickness; ASTM D-638 |
Chevron Phillips EA3350 Crystal Polystyrene
(discontinued **) High heat crystal polystyrene.Applications:Medical containersBlends with clear SB-copolymersClam-shell containersBi-axially oriented sheetFeatures:High molecular weight homopolymerHigh Vicat softeni.. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® C7230P PC+ABS (Asia Pacific) Cycoloy* C7230P resin is a mineral filled, flame retardant PC/ABS. Good stiffness combined with balanced flow and impact performance, makes it a good candidate for various applications. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | 50mm/min; ASTM D638 |
3M Dyneon™ PVDF 6020/1001 Polyvinylidene Fluoride
(discontinued **) Ultra-high molecular weight grade PVDFPowder gradeExcellent chemical resistance to a wide variety of aggressive fluids and solventsGood permeation resistanceExcellent strength and dimensional stabil.. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | ISO 527-1/-2 |
Lanxess Pocan® DP 2004 000000 PBT PBT, non-reinforced, injection molding, halogen free flame retardant |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL RN0401 PPE+PS Noryl RN0401 resin is an unfilled Post Consumer Recycle (PCR) based injection moldable modified polyphenylene ether blend comprising at least 20% PCR content. Available in black only. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL RN0401 PPE+PS (Europe-Africa-Middle East) Noryl RN0401 resin is an unfilled Post Consumer Recycle (PCR) based injection moldable modified polyphenylene ether blend comprising at least 20% PCR content. Available in black only. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DX12411C PC LNP* STAT-KON* DX12411C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Clean Compounding System. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® X4830 PBT+PC Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat .. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | Type I, 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Xylex X7200MR PC+POLYESTER (Asia Pacific) Mold Release version of X7200This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics XYLEX X7300CL PC+POLYESTER PC+ POLYESTER unreinforced alloy developed for optical or lense market. Chemical resistance. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_BFL2200 PC (Europe-Africa-Middle East) design for black light frame application as high flow PC, V-2, high reflection grade. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX GTX974 PPE+PA (Europe-Africa-Middle East) NORYL GTX974 is a material especially designed for in- or on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity for electro-static paintin.. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL HN731SE PPE+HIPS (Europe-Africa-Middle East) PPE+PS blend. For medical devices and pharmaceutical applications. NORYL HN731SE is an unfilled material, with a Vicat B/120 of 135C according ISO 306. Healthcare management of change, biocompati.. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermotuf PK005EI2 PA 6 (Europe-Africa-Middle East) LNP* THERMOTUF* PK005EI2 is a compound based on PA 6 resin containing Impact Modifier, Mineral. Added features include: High Impact.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea.. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | ISO R527 |
Hexcel® HexPly® ES/EH 84 120°C Curing Epoxy Matrix HexPly® ES/EH 84 matrix is a structural epoxy resin for tubular parts designed for low pressure curing in the manufacture of sports goods and for industrial applications. It is ideal for the follow.. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | ASTM D638 |
A. Schulman POLYFORT™ FPP 1080 Glass Fiber-Reinforced Homopolymer Polypropylene DescriptionPolyfort® FPP 1080 is a 20% fiber-reinforced homopolymer polypropylene with excellent strength and heat resistance. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | 50 mm/min; ISO 527 |
CP-Polymer-Technik Wellamid® 6600 HW Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® FG101L NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66 with Developed for Food Contact ApplicationsZytel FG101L NC010 is a lubricated polyamide 66 resin for injection molding. It has been developed for consideration into applic.. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | ISO 527 |
Eurotec® Tecodur® PB70 BK001 HS PBT, unfilled, heat stabilized, black Information provided by Eurotec® |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 103HSL NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103HSL NC010 is a heat stabilized lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | 50 mm/min; ISO 527 |
Eurostar Staramide BST03 PA6, Impact Modified, Injection Molded BST03 is an Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | ISO 527-2 |
Ascend Performance Materials Vydyne® 21SPC Nylon 66, Conditioned Vydyne® 21SPC is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding fabrication. This resin offers a well balanced combination of engineering .. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | ISO 527-1/-2 |
Mitsubishi Xantar® MX 1004 Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances wher.. |
|||
Tensile Strength, Yield | 55.0 MPa | 7980 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® X5600WX PC+POLYESTER (Asia Pacific) Unreinforced, opaque Polyester+PC alloy. Chemical resistance, dimensional stability and mechanical performance. UV Stabilized. Mold ReleaseThis data was supplied by SABIC-IP for the Asia Pacific reg.. |