Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 54.4 MPa | 7890 psi | chs 0.2 in/min; ASTM D638 |
Diamond Polymers Centrex® 925 Injection Molding Grade Centrex 925 resin is a soft-flow, high-gloss, molding grade of Polycarbonate / ASA (acrylonitrile-styrene-acrylate) blend. It is an injection molding grade with a good balance of physical properties.. |