Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 538 MPa @Strain 0.200 %, Temperature 871 °C |
78000 psi @Strain 0.200 %, Temperature 1600 °F |
|
Haynes R-41 alloy, 1.27 mm thick sheet, solution heat treated at 1079°C, water quenched, 30 minutes at 1066°C, aged 16 hours at 760°C (1400°F), air cooled Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ.. |
|||
Tensile Strength, Yield | 538 MPa | 78000 psi | |
Universal Wire Works 90SB-3 Steel Welding Wire Universal 90SB-3 is a 2.25% chromium and 1% molybdenum alloy for welding on steel of similar composition. This alloy is designed for joints in process piping systems, boilers, or pressure vessels. W.. |
|||
Tensile Strength, Yield | 538 MPa | 78000 psi | |
Universal Wire Works 90SB-3L Steel Welding Wire The 90SB-3L alloy is the same as the 90SB-3 alloy with the exception of a restricted carbon content. Universal 90SB-3 is a 2.25% chromium and 1% molybdenum alloy for welding on steel of similar comp.. |
|||
Tensile Strength, Yield | >= 538 MPa | >= 78000 psi | |
Eagle Brass 18665 MSP1, Spring MSP-1 high performance copper alloy with magnesium has high conductivity (63% IACS), high strength and excellent thermal creep properties. Typical uses include terminals, connectors, relays, springs.. |
|||
Tensile Strength, Yield | 538 - 655 MPa | 78000 - 95000 psi | 0.2% offset |
Eagle Brass 521 Phosphor Bronzes 8% C, Hard Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical.. |
|||
Tensile Strength, Yield | 538 - 689 MPa | 78000 - 100000 psi | 0.2% offset |
Eagle Brass 64725 MAX251C, Hard Max 251c has an excellent balance in hardness, formability and conductivity. Typical uses include lead frames, circuit breakers, connectors, electrical springs, contact terminals, and fuse clips.In.. |
|||
Tensile Strength, Yield | 538 - 607 MPa | 78000 - 88000 psi | 0.2% offset |
Eagle Brass 715 Copper Nickel 30%, Extra Hard 715 exhibits excellent corrosion resistance, especially in marine applications. It has moderately high strength and has good creep resistance at elevated temperatures. The cost is relatively high co.. |
|||
Tensile Strength, Yield | 538 - 641 MPa | 78000 - 93000 psi | 0.2% offset |
Eagle Brass 725 Copper Nickel Tin, Extra Hard Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
Tensile Strength, Yield | >= 538 MPa | >= 78000 psi | 0.2% offset |
Eagle Brass 735 Nickel Silver 18%, Extra Spring 735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company |
|||
Tensile Strength, Yield | 538 MPa @Strain 0.200 %, Temperature 566 °C |
78000 psi @Strain 0.200 %, Temperature 1050 °F |
|
Carpenter Custom 450® Stainless Steel, Condition H950 (Age Hardened 510°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
Tensile Strength, Yield | 538 MPa | 78000 psi | |
Universal Wire Works 122 Nickel Alloy Welding Wire Alloy 122 is used for welding of nickel-chromium-molybdenum alloys as well as for overlay cladding on carbon, low alloy, or stainless steels. Alloy 122 is often used on dissimilar joints between nic.. |