Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 526 MPa @Strain 0.200 % |
76300 psi @Strain 0.200 % |
|
Kennametal Stellite Stellite® 31 PM cast Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw cutter inserts, miscellaneous we.. |