Polymer Property : Tensile Strength, Yield = 754 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 5.20 MPa
754 psi
ASTM D412
Precision Polymer Engineering F80X Fluorosilicone Rubber
Mid-Blue Fluorosilicone Rubber, 76-85 °IRHD . Fluorosilicone rubber having methyl, vinyl and fluorine substituent groups on the polymer chain. To meet Aerospace Specification Mil-R-25988B, Class 1,..
Tensile Strength, Yield 5.20 MPa
754 psi
-20% change after 70 hours @ 200°C; ASTM D412
Precision Polymer Engineering S80D Silicone Rubber
Black Silicone Rubber, 76-85 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ. Formulated to meet UK Ministry of Defence ..
Tensile Strength, Yield 5.20 MPa
754 psi
M100
3M Dyneon™ Fluorel™ FT-2320 Fluoroelastomer VF2 + HFP + TFE Terpolymer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 69%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. 69% F grade terpolymer for difficult ex..
Tensile Strength, Yield 5.20 MPa
754 psi
Dow AFFINITY™ SE 1400 Polyolefin Plastomer
AFFINITY® SE 1400 polyolefin plastomer is an ethylene octene resin that offers excellent performance for profile extrusion of thick tubes and good melt strength for low shear blow molding. It has e..
Tensile Strength, Yield 5.20 MPa

@Strain 300 %
754 psi

@Strain 300 %
ASTM D412
Clariant Renol PURSP0002 Polyurethane Elastomer, Ether Based
Data provided by Clariant Masterbatches
Tensile Strength, Yield 5.20 MPa
754 psi
ACC QM260 Addition Cure 2-Part Molding Rubber
Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: cures at room temperature, low shrinkage, high tear and tensile strengths. Applications: expanded PU foam, large obje..
Tensile Strength, Yield 5.20 MPa
754 psi
cured 60 mins @ 100°C
ACC QSil 216 QSI Quantum Silicones Transparent Liquid Silicone Rubber
QSil 216 is a two-part, clear, liquid silicone which will cure at room temperature or at elevated temperatures. It has a low viscosity, which allows for ease of flow around complex parts, providing ..