Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 50.0 MPa | 7250 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Cycolac® G366 ABS (Europe-Africa-Middle East) CYCOLAC G366 is a "new technology" grade of ABS exhibiting outstanding property balance, a good flow, medium impact, medium to high heat resistant and an excellent stability during injection mouldin.. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® C6200 PC+ABS (Europe-Africa-Middle East) CYCOLOY C6200 is a non-chlorinated, nombrominated flame retardant PC/ABS offering balanced heat, flow and impact to meet various application needs. C6200 has improved processing window and edge crac.. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® RCM6123 PC+ABS (Asia Pacific) Cycoloy* RCM6123 resin is an injection moldable filled PC/ABS blend with non-brominated and non-chlorinated flame retardant. It contains 30% post consumer recycle content with a UL-94 V0 rating @ 1.. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | ISO 527 |
SABIC Innovative Plastics LNP FARADEX NS003 PC+ABS (Asia Pacific) LNP* Faradex* NS003 is a compound based on PC+ABS Blend resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | ISO 527 |
Eastman Eastar GN005 Copolyester, Natural
(discontinued **) Eastar GN005 Copolyester is a glycol modified polyethylene terephthalate (PET) with an added mold release. Eastar GN005 copolyester will not crystallize and thus offers wider processing latitude tha.. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | 50 mm/min |
Eastman Eastalloy DA111 PC+PET Copolyester/Polycarbonate
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Tensile Strength, Yield | 50.0 - 70.0 MPa | 7250 - 10200 psi | Injection; ISO 527 |
Raschig Group SURAPLAST UPA 63 UP Glass fiber reinforced polyester molding compound. Minimal mold shrinkage and post-shrinkage, very good arc resistance, very good mechanical strength. This product meets the allowed upper limits for.. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | 5 [mm/min], Test Speed 50 [mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® S31 (3484) PA 6.10 Conditioned
(discontinued **) A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | ISO 527-1/-2 |
Kuraray Genestarâ„¢ N1001D-U83/02 Nylon Standard unreinforced extrusion grade. Main Features:Outstanding fuel barrierHeat resistanceExample of applications:Multi-layered fuel tube |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP QAP22S PA 6/10 (Asia Pacific) LNP* Lubricomp* QAP22S is a compound based on Nylon 6/10 resin containing PTFE, Aramid Fiber, Silicone. Added features of this material include: Internally Lubricated, Heat Stabilized. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 357X PBT (Europe-Africa-Middle East) VALOX 357X is an impact modified, flame retarted PBT+PC blend. Applications like bobbins, switches and enclosures. |
|||
Tensile Strength, Yield | 50.0 - 60.0 MPa @Thickness 2.00 mm |
7250 - 8700 psi @Thickness 0.0787 in |
50 mm/min; ASTM D638 |
Solvay Specialty Polymers Solef® 1006 Polyvinylidene Fluoride (PVDF) Solef® 1006 PVDF is a very low viscosity homopolymer resin mainly used in injection molding or in multifilament extrusion.Features: Homopolymer; Low ViscosityUses: General PurposeAdditional Prope.. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® 5220U PBT+PC Unreinforced PBT+PC Alloy. Impact Modified. Improved retention of mechanical properties under UV exposure. Excellent low temperature impact and chemical resistance. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® BF-0670T MABS, Unreinforced Scratch Resistant Scratch resistant material that is used in the exterior of electric products and household appliancesInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® LX-0971 S ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL GTX GTX974 PPE+PA (Europe-Africa-Middle East) NORYL GTX974 is a material especially designed for in- or on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity for electro-static paintin.. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Noryl GTX LMX171 PPO/PBT (Europe-Africa-Middle East) Noryl LMX171 is a PPO/PBT blend including conductive agent with a balanced heat/impact property profile. Noryl LMX differentiate from Noryl GTX by a lower moisture uptake (0.15%).This data was suppl.. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | ASTM D638 |
A. Schulman POLYFORT™ FPP 1220 Glass Filled Chemically Coupled Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1220 is a 20% glass filled chemically coupled impact copolymer polypropylene product.Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | ASTM-D638 |
Polyram RamShine PVS701 AES, UV Stabilized UV stabilized injection molding AESInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | ISO R527 type 1 |
Hexcel® HexPly® 916 120°C Curing Epoxy Matrix HexPly® 916 is a self-extinguishing modified epoxy matrix system with very high self adhesive properties. It is an ideal system for single shot honeycomb sandwich manufacture, with good drape chara.. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | ASTM D 638 |
Cossa Polimeri ESTABLEND 4500 V0 HF Flame Retardant PC - ABS PC - ABS BlendFlame retardant class V0, chlorine and bromine free, good light resistance, excellent mechanical properties, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | parallel; ISO 527-3 |
Covestro Desmopan® 3385A Polyurethane Extrusion- and injection molding gradegood wear resistanceshort cycle timeshigh melt stabilityApplicationhard - soft systemsHosesnon-reinforcedProfilesInjection molded engineering partsPreprocessing.. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | dry; ISO 527-1/-2 |
DSM Novamid® ST220 NAT PA6-I Impact Modified, Injection Molding, Medium Viscosity |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® R 50 H NZ PA6 Product description: Grilon R 50 H NZ is a high viscosity, unreinforced, heat stabilized, impact modified PA6 extrusion blow molding grade. Grilon R 50 H NZ has the following important properties: V.. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | ISO 527 |
Clariant Renol PA1SP0003 Nylon 66, PE Modified Reduced Coefficient of FrictionData provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | Conditioned; ISO R 527 |
Addiplast Addinyl C2 Nylon 66/6 Unreinforced, medium viscosityInformation provided by Addiplast. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | ISO 527-2 |
Ascend Performance Materials Vydyne® 41H Nylon 66, Impact Modified, DAM Vydyne® 41H is a general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne.. |
|||
Tensile Strength, Yield | 50.0 MPa | 7250 psi | 50 mm/min; ISO 527 |
CP-Polymer-Technik Wellamid® 6000/58 CP Nylon 6, Impact Modified Until -40°C, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |