Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 0.500 MPa | 72.5 psi | 70°C for 1,000 hrs; JIS-K-6251(#2) |
Fujipoly Industries Sarcon® GR-c Gap Filler Pad Sarcon GR-c is a highly conformable, thermally conductive (no electric conductive) and electromagnetic wave absorption material in areas where space between surfaces is uneven and surface textures v.. |
|||
Tensile Strength, Yield | 0.500 MPa | 72.5 psi | JIS-K-6251(#2)/ASTM D-412 |
Fujipoly Industries Sarcon® GR-Fd Gap Filler Pad Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-Fd has a mesh embedded overall.Information provided b.. |
|||
Tensile Strength, Yield | 0.500 MPa | 72.5 psi | 150°C for 1,000 hrs; JIS-K-6251(#2) |
Fujipoly Industries Sarcon® GR-HFd Gap Filler Pad Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-HFd has a hardened top surface and mesh embedded over.. |
|||
Tensile Strength, Yield | 0.500 MPa | 72.5 psi | 150°C for 1,000 hrs; JIS-K-6251(#2) |
Fujipoly Industries Sarcon® GR-m Gap Filler Pad Sarcon GR-m is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Tensile Strength, Yield | 0.500 MPa | 72.5 psi | JIS-K-6251(#2)/ASTM D-412 |
Fujipoly Industries Sarcon® GR-Hd Gap Filler Pad Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-Hd has a hardened top surface.Information provided by.. |
|||
Tensile Strength, Yield | 0.500 MPa | 72.5 psi | |
ACC MM709 Low Tear Condensation Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: low viscosity, good resistance to styrene attack, easy degassing, low shrinkage, range of catalysts. Applications: sh.. |