Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 492 MPa @Strain 0.200 % |
71400 psi @Strain 0.200 % |
|
Haynes Hastelloy® C-4 alloy, all-weld metal, as welded, GTAW Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang.. |