Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 49.03 MPa @Thickness 3.20 mm |
7112 psi @Thickness 0.126 in |
Type 1, 5 mm/min; ASTM D-638 |
Bhansali Engineering Abstron AN480V2 Flame Retardant ABS Grade Information provided by Bhansali |
|||
Tensile Strength, Yield | 49.03 MPa @Thickness 3.20 mm |
7112 psi @Thickness 0.126 in |
Type 1, 5 mm/min; ASTM D-638 |
Bhansali Engineering Abstron IMC-45 FR V2 Flame Retardant PC/ABS Grade Information provided by Bhansali |
|||
Tensile Strength, Yield | 49.03 MPa @Thickness 3.20 mm |
7112 psi @Thickness 0.126 in |
Type 1, 5 mm/min; ASTM D-638 |
Bhansali Engineering Abstron AN480V2 Flame Retardant ABS Grade Information provided by Bhansali |
|||
Tensile Strength, Yield | 49.03 MPa @Thickness 3.20 mm |
7112 psi @Thickness 0.126 in |
Type 1, 5 mm/min; ASTM D-638 |
Bhansali Engineering Abstron IMC-45 FR V2 Flame Retardant PC/ABS Grade Information provided by Bhansali |